连铸保持了细粒度、致密的铸态结构. 铁棒从坩埚的底部拉出,使所有的渣滓, 炉渣和其他杂质浮到炉顶. 这一过程使产品适合于要求严格符合公差的应用, 机械加工性能好,强度高.
连续铸铁提供了更细的石墨,并改善了机械性能. Continuous cast iron properties allow you to machine a great variety of parts faster and with less waste; thus higher profitability.
年级/形状 |
Min () |
Max () |
马克斯(宽度) |
长度(英尺) |
---|---|---|---|---|
65-45-12迪路 | 1.5 | 6 | 5 to 6 | |
80-55-16迪路 | 2.25 | 8 | 5 to 6 | |
g2 AC公寓 & SQ | 0.75 | 4.25 | 5 to 6 | |
g2 AC RD | 0.625 | 12 | 5 to 6 |